Vertical foundation cracks in poured concrete are usually shrinkage and often harmless if they're thin and not growing. Horizontal foundation cracks in basement walls are the most serious type, usually caused by soil pressure pushing the wall inward. Stair-step cracks in block or brick suggest settling. Any crack wider than about 1/4 inch, growing, leaking, or with one side offset should be looked at by a professional.
Almost every foundation cracks. Concrete shrinks as it cures, and the result is often a thin vertical crack in the first year or two. The skill is reading the crack: its direction, width, shape, and whether it's still moving.
Foundation crack types at a glance
| Crack | Usual cause | Concern level |
|---|---|---|
| Hairline vertical (poured concrete) | Shrinkage during curing | Low; monitor, seal if it leaks |
| Vertical, wider at one end | Settling of one section | Moderate; monitor or inspect |
| Diagonal (often from corners) | Differential settling | Moderate to high |
| Horizontal (basement wall) | Soil and water pressure | High; get it inspected |
| Stair-step (block or brick) | Settling or lateral pressure | Moderate to high |
| Corner crack (small, at the top corner) | Slab/wall movement, temperature | Usually low |
Vertical foundation cracks
The most common type. In poured concrete walls they usually come from shrinkage and are typically thin and uniform in width. Concern rises when a vertical crack is wider at the top or bottom, has one side pushed in or out further than the other, or lets water in. A leaking vertical crack is usually fixed with crack injection.
Horizontal foundation cracks
A horizontal crack in a basement wall usually means soil outside is pushing on the wall, often from water-saturated or expansive clay. It's the type most likely to come with bowing. A horizontal crack in a basement wall should be evaluated professionally regardless of width. See bowing basement walls.
Cracks in block foundations
Cracks in block foundations often follow the mortar joints, either in a stair-step pattern (settling) or horizontally along a joint about halfway up the wall (pressure). Blocks themselves cracking is more serious than mortar-joint cracks.
Hairline cracks in the foundation
A hairline crack, less than about 1/16 inch, that isn't leaking and isn't growing is usually cosmetic. Mark it, date it, and check it seasonally. Seal it if it lets moisture in.
Corner cracks in the foundation
Small diagonal cracks at the top corners of a poured wall, or where a slab meets a wall, are common and often caused by temperature and shrinkage. They're usually minor unless they widen or come with other signs.
How wide is too wide?
| Width | Rough guide |
|---|---|
| Under 1/16 inch | Usually cosmetic |
| 1/16 – 1/8 inch | Seal and monitor |
| 1/8 – 1/4 inch | Warning; measure monthly |
| Over 1/4 inch | Professional evaluation |
Source: US Waterproofing. Angi suggests a lower trigger: cracks wider than 1/8 inch or raised on one side could indicate structural damage and need professional attention.
Take a photo of each crack with a coin next to it, every three months. Comparing photos side by side is the simplest way to tell a stable crack from a growing one.
What foundation crack repair costs
Non-structural crack injection usually costs $250 to $800 per crack, while structural crack repairs run $1,000 to $5,000 for minor work and $10,000 to $30,000+ for major repairs (HomeGuide). See foundation crack repair for methods.
Crack width guide
| Width | Common meaning |
|---|---|
| Hairline (under about 1/16") | Usually shrinkage |
| 1/16" to 1/8" | Monitor; seal if leaking |
| 1/8" to 1/4" | Worth an assessment, especially if growing |
| Over 1/4" | Likely movement; get it evaluated |
| Any width with displacement | Movement; get it evaluated |
Angi notes that cracks wider than 1/8 inch or raised on one side could indicate structural damage (Angi).
Poured concrete vs block foundation cracks
- Poured concrete typically cracks vertically or diagonally from shrinkage and settlement. Horizontal cracks are a warning sign of soil pressure.
- Block foundations crack along mortar joints, often as stair-steps at corners or a horizontal line mid-wall when soil pushes in.
See cracks in block foundations and stone and bowing basement walls.
What to tell a contractor on the first call
- Foundation type (poured, block, slab, pier and beam).
- Crack direction, width and length, and whether it leaks.
- How long it's been there and whether it's growing.
- Any other signs: sticking doors, sloping floors, bowing.
- Photos with a ruler for scale.
Frequently asked questions
Are vertical foundation cracks normal?
Thin, uniform vertical cracks in poured concrete are usually shrinkage and common. Wider cracks, offset cracks or leaking cracks need attention.
Why are horizontal foundation cracks serious?
They usually mean soil and water pressure are pushing the wall inward, which can lead to bowing and, left alone, wall failure.
Do hairline cracks in a foundation need repair?
Usually not structurally, if they're not growing. Seal them if they let in water, and monitor them.
When should I call someone about a foundation crack?
When it's horizontal, wider than about 1/4 inch, growing, leaking, has one side offset, or comes with sticking doors or sloping floors.
Can foundation cracks be cosmetic?
Yes. Many hairline vertical cracks in poured concrete are cosmetic shrinkage cracks. Width, direction, displacement and growth decide whether they're structural.
Do all foundation cracks need to be repaired?
No. Non-leaking hairline cracks can simply be monitored. Leaking cracks are usually sealed; structural cracks need a repair plan.
Foundation cracks are common, and most aren't dangerous, but the wrong kind is worth catching early. Call the number on this page to reach a participating local foundation repair company.
Written and fact-checked by DryLevel editors, last updated 2026-11-16. Costs come from the sources linked in the article. Read our editorial policy or report a correction.